PLA
Models, prototypes, desk items, fit checks.
Values from the Bambu Lab PLA Basic, Technical Data Sheet V3.0. Open the original PDF ↗
- Softens at
- 57 °C
- Strength, flat
- 35 MPa
- Strength, upright
- 31 MPa
- Water uptake
- 0.43%
About this grade
PLA is the most common material in 3D printing as it’s easy to print and inexpensive. Its stiffness and strength can meet most printing needs. Bambu PLA Basic is designed for high-speed printing and has excellent toughness and Z-layer strength.
Not the best choice for
Anything that gets warm, like a car in summer or a part near a motor. It softens from about 55 °C.
Jet black, Bone white, Slate grey, Molto orange, Racing green, Cobalt, Sunflower, Signal red
Physical properties
| Property | Test | Value |
|---|---|---|
| Density | ISO 1183 | 1.24 g/cm³ |
| Melting temperature | DSC, 10 °C/min | 160 °C |
| Glass transition temperature | DSC, 10 °C/min | 60 °C |
| Vicat softening temperature | ISO 306 | 57 °C |
| Heat deflection temperature | ISO 75, 1.8 MPa | 54 °C |
| Heat deflection temperature | ISO 75, 0.45 MPa | 57 °C |
| Saturated water absorption | 25 °C, 55% RH | 0.43% |
Mechanical properties
| Property | Test | Printed flat (X-Y) | Printed upright (Z) |
|---|---|---|---|
| Young’s modulus | ISO 527 | 2580 ± 220 MPa | 2060 ± 170 MPa |
| Tensile strength | ISO 527 | 35 ± 4 MPa | 31 ± 3 MPa |
| Elongation at break | ISO 527 | 12.2 ± 1.8% | 7.5 ± 1.3% |
| Bending modulus | ISO 178 | 2750 ± 160 MPa | 2370 ± 150 MPa |
| Bending strength | ISO 178 | 76 ± 5 MPa | 59 ± 6 MPa |
| Impact strength | ISO 179 | 26.6 ± 2.8 kJ/m² | 13.8 ± 0.9 kJ/m² |
| Impact strength, notched | ISO 179 | 7.9 ± 1.2 kJ/m² | – |
Chemical resistance
| Acids | Not resistant |
|---|---|
| Alkalis | Not resistant |
| Organic solvents | Not resistant to some organic solvents |
| Oil and grease | Resistant to most kinds of oil and grease |
| Flammability | Flammable |
Manufacturer's print settings
| Nozzle sizes | 0.2, 0.4, 0.6, 0.8 mm |
|---|---|
| Nozzle temperature | 190–230 °C |
| Bed temperature | 35–45 °C |
| Chamber temperature | 25–45 °C |
| Drying | 50 °C for 8 h |
| Max overhang angle | 55° |
| Max bridging length | 30 mm |
How the test bars were made: Printed at 220 °C nozzle, 35 °C bed, 200 mm/s and 100% infill, then annealed and dried at 55 °C for 8 h before testing. These are typical values for solid test bars, for comparing materials. A real part's strength also depends on its shape, infill and which way it was printed. Source: Bambu Lab PLA Basic, Technical Data Sheet V3.0.